Balanced Alloy Steel Chemistry for Optimum Hardness/Toughness Ratio
-
Quenched & Tempered, thru-hardened up to 2"
-
418-495 BHN, Average 450 BHN
Used in applications where extreme shock and abrasive wear are the primary cause of failure. Excellent weldability, formability, and Machining properties.
 |
 |
Chemical Composition / Typical Mechanical Properties |
 |
 |
 |
 C
 |
 |
 M
 |
 |
 P
 |
 |
 S
 |
 |
 Si
 |
 |
 Ni
 |
 |
 Cr
 |
 |
 Mo
 |
 |
 Ti or Va
 |
 |
 Cu
 |
 |
 B
 |
 |
 |
 |
 0.22 / 0.26
 |
 |
 0.70 / 1.00
 |
 |
 0.025 max
 |
 |
 0.010 max
 |
 |
 0.15 / 0.40
 |
 |
 0.40 / 0.70
 |
 |
 1.25 / 1.75
 |
 |
 0.20 / 0.30
 |
 |
 0.04 / 0.10
 |
 |
 0.35 max
 |
 |
 0.0015 / 0.005
 |
 |
 |
 |
 |

Tensile strength (ksi)
 |
 |

Yield strength (ksi)
 |
 |

Elongation in 2"
 |
 |

Charpy V-Notch Room Temp.
 |
 |

Reduction of Area
 |
 |
 |
 |
 225/235
 |
 |
 180/190
 |
 |
 11/12%
 |
 |
 18/28
 |
 |
 40/42%
 |
 |
 |
Product Information
Welding Guidelines
Machining
Forming
Heat Treating
Cutting
Printable Specs Sheet
|
 |